Deposition of 100 nm thickness to 32 aspect ratio hole
The result shows the bottom of the hole. In addition, the top, sides, and bottom of the film are all coated with a thickness of 100 nm, enabling the ALD to achieve a uniform film thickness.
The result shows the bottom of the hole. In addition, the top, sides, and bottom of the film are all coated with a thickness of 100 nm, enabling the ALD to achieve a uniform film thickness.